PUR-Resin (Polyol) | PUR-Hardener (Isocyanate) | Key Properties | Applications | Download TDS |
|---|
PR-3600 | PH-3900 | - simulates rubber
- shore A 80
| Functional prototype parts, short run production, Rapid Prototyping | |
| PH-3904 | - simulates rubber
- shore A 65-70
- high elongation at break
- fast demold time
| |
PR-3602 | PH-3904 | - Simulates PE/PP
- very good impact resistance
- fast demold time
| Functional prototype parts & bumpers, short run production, Rapid Prototyping | |
| PH-3905 | - simulates PE/PP
- good impact strength
- temperature resistant (90 °C)
- fast demold time
| |
PR-3603 | PH-3904 | - simulates PP / ABS
- short demold time
- good elastic memory
- Shore D75-80
| Functional prototype parts, short run production, rapid prototyping | |
| PH-3905 | - simulates PP / ABS
- short demold time
- good elastic memory
- Shore D75-80
| |
PR-3608 | PH-3905 | - simulates PP / ABS
- short demold time
- temperature resistant (130-135 ºC)
- Shore D 75-80
| Functional prototype parts, short run production, rapid prototyping | |
PR-3652 | PH-3905 | - simulates PP / ABS
- short demold time
- temperature resistant (130 ºC)
- glass fiber filled
- Shore D 75-80
| Functional prototype parts, short run production, rapid prototyping | |
PR-3654 | PH-3905 | - simulates PP / ABS
- short demold time
- temperature resistant (130 ºC)
- glass fiber filled
- Shore D 80-85
| Functional prototype parts, short run production, rapid prototyping | |